Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Terblend S" in Material Data Center leads to the following information:

Tradename: Terblend S
Family: ASA+PA
Producer: INEOS Styrolution
2 hits in the material database
3 hits in the literature database
1 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Styrene Copolymers (ABS, ASA, SAN)
...) [1]. Even after BASF's takeover of the styrene copolymer business from DSM, the brand name Ronfalin will continue. In ABS blends, seven different products from four manufacturers are significant on the market (Table 2). Blends with PC include Terblend S (BASF), Bayblend (Bayer), Pulse (Dow) and Cycoloy and Geloy (GE Plastics). (PA+ABS) blends are marketed by BASF as Terblend N and by Bayer as Triax. Market Segments Thanks to their versatile applications and processing properties, styrene...

Kunststoffe international, 2011-10-17, Styrene Copolymers (ABS, ASA, SAN, MABS, and ABS Blends)
...facturing light colored parts that are required to offer color fastness and constancy over relatively long periods. Styrolution recently expanded its portfolio of styrene copolymers with a new variant of the material (Terblend S), which is impressive for its further improved UV stability. Potential applications are those with high light exposure, such as automotive interiors (e.g. rear shelves) and parts of gardening equipment. The material is currently in the sampling phase. Outlook The commodi...

Kunststoffe international, 2014-10-10, Styrene Copolymers
Styrene polymers continue to maintain their position in the global market due to continuous advances and innovations. The sharp surge in demand for specialty copolymers has led to an increase in production capacity by the producers in Asia and the Middle East. The rise of demand will go on. ABS standard and polymersCapacity (kt/a)Market development (kt/a)20119,2007,15020129,9007,120201310,3007,350Developments in processes, products and applications for styrene polymers are being systematically ...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.